Used welded pipe production line, the cause of the nozzle defect after the flying saw is disconnected?

Used welded pipe production line, the cause of the nozzle defect after the flying saw is disconnected?

  • Sort:Information
  • Auth:
  • Source:
  • Release time:2021-10-20 12:00
  • Pvs:

【概要描述】Types of nozzle defects in the used welded pipe production line: nozzle defects mainly include flattened, oblique, rubbed, and blocked nozzles.

Used welded pipe production line, the cause of the nozzle defect after the flying saw is disconnected?

【概要描述】Types of nozzle defects in the used welded pipe production line: nozzle defects mainly include flattened, oblique, rubbed, and blocked nozzles.

  • Sort:Information
  • Auth:
  • Source:
  • Release time:2021-10-20 12:00
  • Pvs:
Detail

Types of nozzle defects in the used welded pipe production line: nozzle defects mainly include flattened, oblique, rubbed, and blocked nozzles.

Analyze nozzle defects of used welded pipe production line

 

Deflated head defect

 

Used welded pipe production line

 

Shrinking heads mostly occur on thin-walled tubes. The fundamental reason is that the tube wall is thin and the ability to resist the impact of the saw blade is weak. The specific reasons are as follows:

(1) The saw blade has been used for too long, and the saw tooth wear is more serious;

(2) The thickness of the saw blade is not well chosen, and it is too thick;

(3) The pressure of the sawing cylinder is too large.

 

Oblique head defect

 

Used welded pipe production line

 

Main reasons for oblique head:

(1) The flying saw is not synchronized with the welded pipe.

(2) There is radial vibration in the bearing of the sawing spindle.

(3) The saw blade shakes greatly.

(4) The operation of the sawing trolley is unstable.

 

Wiping defects

 

Used welded pipe production line

 

Main reasons for head rubbing:

(1) Improper design of main parameters of lifting saw;

(2) The design plan for the main parameters of the loose clamp is too early

(3) There is axial shaking of the sawing spindle bearing

 

Nozzle blocking defect

 

Used welded pipe production line

 

Main reasons for nozzle blockage:

(1) Different steps;

(2) The saw blade shakes a lot;

(3) There is radial sway on the back of the saw;

 

The above is used welded pipe production line, the cause of the nozzle defect after the flying saw is disconnected. I hope it will be of some help to you.

 

Part of the content of this site comes from the Internet. This site only provides information storage. The copyright belongs to the original author. It does not bear the relevant legal responsibility and does not represent the views and positions of this site. Please contact and delete it if there is any infringement.

关键词:

More News

Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (1)
Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (1)
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me introduce the solution to the difficult forming of thick-walled tube(1).
Detail
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me introduce the solution to the difficult forming of thick-walled tube(1).
Analyzing the roll life of a used ERW tube mill
Analyzing the roll life of a used ERW tube mill
In the production of used ERW tube mills, the roll is the key and important special tool. Roll consumption is also a key tool for manipulating product costs. In addition, the normal operation of the roll will directly affect the output and quality of welded pipe manufacturing. Therefore, welded pipe manufacturers attach great importance to and strive to improve the service life of the roll.
Detail
In the production of used ERW tube mills, the roll is the key and important special tool. Roll consumption is also a key tool for manipulating product costs. In addition, the normal operation of the roll will directly affect the output and quality of welded pipe manufacturing. Therefore, welded pipe manufacturers attach great importance to and strive to improve the service life of the roll.
How to extend the service life of high frequency welded pipe equipment
How to extend the service life of high frequency welded pipe equipment
The service life of high frequency welded pipe equipment is of concern to everyone. The contribution made in the welding industry is immeasurable, and the care of it by customers should be paid more attention. So how can the service life of high frequency welded pipe equipment be extended in the actual production process?
Detail
The service life of high frequency welded pipe equipment is of concern to everyone. The contribution made in the welding industry is immeasurable, and the care of it by customers should be paid more attention. So how can the service life of high frequency welded pipe equipment be extended in the actual production process?
Adjusting the welding seam position of square and rectangular pipes made by directly forming to square pipe mill (2)
Adjusting the welding seam position of square and rectangular pipes made by directly forming to square pipe mill (2)
Judging that the quality of the square tube produced by the directly forming to square pipe mill meets the standard is based on a large number of inspection data of the microhardness of the weld and the microhardness of the base material. The former is much higher than the latter. It is for this reason that the weld is usually not placed at a positive angle, but placed within t~(t+5mm) from the corner edge to reduce the risk of weld cracks. This requires effective control of the weld position. Control methods include forming roll method, guide roll method and sizing roll method.
Detail
Judging that the quality of the square tube produced by the directly forming to square pipe mill meets the standard is based on a large number of inspection data of the microhardness of the weld and the microhardness of the base material. The former is much higher than the latter. It is for this reason that the weld is usually not placed at a positive angle, but placed within t~(t+5mm) from the corner edge to reduce the risk of weld cracks. This requires effective control of the weld position. Control methods include forming roll method, guide roll method and sizing roll method.
Contact information
Tel: +86-13392281699
Wechat: 13392281699
Email: zty@usedpipemill.com
Company address:No. A99, East Lecong Avenue, Lecong Town, Foshan City, Guangdong Province

Recommendation

Online Inquiry

留言应用名称:
底部留言
描述:

LINK

Contact Us

Tel (wechat): 13336487288
Wechat:+86 13336487288

WhatsApp:+86 13336487288
Email: zty@usedpipemill.com

Address: No. A99, Lecong Avenue East, Lecong Town, Foshan City, Guangdong Province

QRCODE

Copyright 0 2021 jinyujie. 粤ICP备13051810号 Powerby:  300.cn