【概要描述】The dominant defects of the welded tube blank of the high frequency welded pipe machine generally include cracked edges, broken edges, sawtooth, pitting, scratches, roll marks, dark spots, edge burrs, sickle bends, wrinkles, waves, edge warping, and points. Layers, warped skins, pinholes, sticky rolls, soft spots, rust, oxide layers, towers, loose rolls, etc. Let me introduce you to the causes of cracked edges and the effect of cracked edge billets on welded pipes.

About the influence of the defects of the welded pipe blank of the high frequency welded pipe machine on the quality of the welded pipe (5)

【概要描述】The dominant defects of the welded tube blank of the high frequency welded pipe machine generally include cracked edges, broken edges, sawtooth, pitting, scratches, roll marks, dark spots, edge burrs, sickle bends, wrinkles, waves, edge warping, and points. Layers, warped skins, pinholes, sticky rolls, soft spots, rust, oxide layers, towers, loose rolls, etc. Let me introduce you to the causes of cracked edges and the effect of cracked edge billets on welded pipes.

  • Sort:Information
  • Auth:
  • Source:
  • Release time:2022-09-28 11:30
  • Pvs:
Detail

If the high frequency welded pipe machine refers to the chemical composition and mechanical properties of welded tube blanks that require certain inspection methods to be known as invisible defects; then, those defects that can be seen only by vision are called tube blanks. Overt defect.

 

The dominant defects of the welded tube blank of the high frequency welded pipe machine generally include cracked edges, broken edges, sawtooth, pitting, scratches, roll marks, dark spots, edge burrs, sickle bends, wrinkles, waves, edge warping, and points. Layers, warped skins, pinholes, sticky rolls, soft spots, rust, oxide layers, towers, loose rolls, etc. Let me introduce you to the causes of cracked edges and the effect of cracked edge billets on welded pipes.

 

High frequency welded pipe machine

 

Causes of burrs and edge warping:

(1) The slitting blade of slitting is not sharp.

(2) The precision of the slitter knife shaft is poor, or there are impurities on the spacer plane, which causes the slitting knife plane to swing on the knife shaft, which affects the side clearance and produces periodic burrs on the edge of the tube blank.

(3) The gap between the upper and lower edges of the slitting blade is too large.

 

The effect of burrs and edge warpage on the quality of welded pipes:

(1) Slight tube blank burrs and edge warping have little effect on thick-walled tubes and standard-walled tubes: for some tubes that require smaller internal burrs and extremely small tubes, you can also reverse the tube blank The feeding method achieves the purpose.

 

(2) When the edge is warped severely, a "corner joint" will be formed, that is, the outer edge corner joint shown in Figure A will appear when the A side is rolled on the outside, and the outer edge corner joint shown in Figure A will appear when the A side is rolled to the inside. The inner edge of the corner joint, the two edge butt forms are undesirable for the welding process.

 

High frequency welded pipe machine

 

(3)The external burrs of thin-walled tubes are difficult to remove. Tube blanks with large edge burrs and warped edges should be avoided as much as possible in the production of thin-walled tubes.

 

About the high frequency welded pipe machine welded tube defects (5) introduction of burrs and edge warping, and the impact of burrs and edge warping on the quality of welded pipes, I hope it can help you.

关键词:

More News

Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (2)
Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (2)
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me first introduce the solution (2) of the fine forming hole pattern .
Detail
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me first introduce the solution (2) of the fine forming hole pattern .
Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (1)
Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (1)
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me introduce the solution to the difficult forming of thick-walled tube(1).
Detail
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me introduce the solution to the difficult forming of thick-walled tube(1).
Solution for thick wall tube forming of used round pipe to square pipe machines(2)
Solution for thick wall tube forming of used round pipe to square pipe machines(2)
In the welded pipe industry, people generally regard welded pipes with a wall thickness to outside diameter (thickness-to-diameter ratio) of 12%≤t/D≤18% as thick-walled pipes. Difficulties in used round pipe to square pipe machines, clearly put forward the adjustment methods of thick-walled tube forming.
Detail
In the welded pipe industry, people generally regard welded pipes with a wall thickness to outside diameter (thickness-to-diameter ratio) of 12%≤t/D≤18% as thick-walled pipes. Difficulties in used round pipe to square pipe machines, clearly put forward the adjustment methods of thick-walled tube forming.
Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (1)
Solutions to difficulties in thick-walled pipe forming of directly forming to square pipe mill (1)
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me introduce the solution to the difficult forming of thick-walled tube(1).
Detail
Solutions to solve the difficulties in forming thick-walled tubes of directly forming to square pipe mill include special forming unit solutions, rough forming pass solutions, fine forming pass solutions and comprehensive solutions. Let me introduce the solution to the difficult forming of thick-walled tube(1).
Contact information
Tel: +86-13392281699
Wechat: 13392281699
Email: zty@usedpipemill.com
Company address:No. A99, East Lecong Avenue, Lecong Town, Foshan City, Guangdong Province

Recommendation

Online Inquiry

留言应用名称:
底部留言
描述:

LINK

Contact Us

Tel (wechat): 13336487288
Wechat:+86 13336487288

WhatsApp:+86 13336487288
Email: zty@usedpipemill.com

Address: No. A99, Lecong Avenue East, Lecong Town, Foshan City, Guangdong Province

QRCODE

Copyright 0 2021 jinyujie. 粤ICP备13051810号 Powerby:  300.cn